Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
|
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-30-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which ena.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-30-20064 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement. Standard available thickness 0.064"Features and Benefits of PORON Products: Excelle.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-30-25047 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-30-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-40-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-40-30 Cellular Urethane Foam Information on this material is preliminary.Standard color is black (04); others are available. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F).General Poron® information: Poron® fo.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-41-15 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-41-20 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-41-30 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-50 Thin as Cast Urethane Foam, Firm, Thin as Cast Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-50-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-50-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-60-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-60-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-60-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4790-92-12 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force.Features and Benefits of PORON Products: Excellent compression set resistance which enables durable, long-term performance for gasketing, seali.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4790-92-20 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which enab.. |
|||
CTE, linear | 230 - 310 µm/m-°C | 128 - 172 µin/in-°F | |
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-40-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
CTE, linear | 230 - 310 µm/m-°C @Temperature 20.0 °C |
128 - 172 µin/in-°F @Temperature 68.0 °F |
ASTM C518 |
Rogers Corporation Poron® 4701-50-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
CTE, linear | 63.0 - 310 µm/m-°C | 35.0 - 172 µin/in-°F | Average value: 214 µm/m-°C Grade Count:39 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |