Polymer Property : CTE, linear = 17.2 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 17.2 µm/m-°C

@Temperature 260 °C
9.56 µin/in-°F

@Temperature 500 °F
Ferro EG 3608 Metal Sealing
Glass Type: Si-Ti Alkali Typical Powder Form: VSD Typical Application: Al Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals fo..
CTE, linear 17.2 µm/m-°C

@Temperature 20.0 - 1000 °C
9.56 µin/in-°F

@Temperature 68.0 - 1830 °F
Goodfellow T1-Thermocouple Alloy
The positive element of the type K thermocouple alloy the negative being T2. The thermocouple can be used up to 1250C in oxidizing atmospheres and is the probably the most common in use. It is also ..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 TB Wire quenched Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 TD2 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 TD4 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 TDX Rod quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 TDX Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 TH1 Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 TH1 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 TH2 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 TH3 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 TH4 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 THX Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 THX Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 TD1 Rod quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 TD1 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 TD3 Wire quenched/Cold Rolled Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
CTE, linear 17.2 µm/m-°C

@Temperature 0.000 - 200 °C
9.56 µin/in-°F

@Temperature 32.0 - 392 °F
CLAL-MSX DECLAFOR® 1015 TF Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..