Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 298 µm/m-°C @Temperature 20.0 °C |
166 µin/in-°F @Temperature 68.0 °F |
Cured property; alpha 2; ASTM E831-86 |
Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound UVISTAKE 7205LM-PMF is a 100% solids, thixotropic, one component, premixed frozen, electrically insulating, urethane system designed for the attachment and staking of electrical/electronic component.. |