Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer Aptek Laboratories
Trade Name UVISTAKE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UVISTAKE 7205LM-PMF is a 100% solids, thixotropic, one component, premixed frozen, electrically insulating, urethane system designed for the attachment and staking of electrical/electronic components mounted on printed circuit boards. This system provides an excellent combination of flexibility and strength for demanding applications where toughness is required for the management of thermomechanical stresses. UVISTAKE 7205LM-PMF will become tack free when exposed to the proper UV light radiation. The staking compound will fully post cure in exposed and shaded areas in 14 days at 25ºC and 50% relative humidity, as an alternative, the post cure for the staking compound in both exposed and shaded areas may be accelerated with low to moderate heat.Multicure mechanism for complete cure in shaded areas underneath components; Good flexibility for reduced stress in the encapsulation of sensitive glass-bodied components; Meets NASA condensable volatile requirements for high vacuum environments; Highly reversion resistant for good physical stability under high heat and humidity environments; Excellent adhesion to plastic/metal components and substrates; More rigid version (95A) available as UVISTAKE 7205-PMF; Packaged in syringes for convenient dispensing; No TDI, no toxic solvents, no free acrylic acid for safetyInformation provided by Aptek Laboratories, Inc.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D1475
Outgassing - Total Mass Loss 0.80 - 2.5 %
0.80 - 2.5 %
Cured property; at 10E-6 torr; ASTM E595
Collected Volatile Condensable Material 0.030 %
0.030 %
Cured property; at 10E-6 torr; ASTM E595
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Cured property; ASTM D2240
Thermal Properties Metric English Comments
CTE, linear 298 µm/m-°C

@Temperature 20.0 °C
166 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 2; ASTM E831-86
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
Cured property; ASTM E831-86
Flash Point >= 100 °C
>= 212 °F
ASTM D92
Electrical Properties Metric English Comments
Volume Resistivity 5.40e+14 ohm-cm
5.40e+14 ohm-cm
Cured property; ASTM D257
Dielectric Constant 3.5

@Frequency 1000 Hz
3.5

@Frequency 1000 Hz
Cured property; ASTM D150
Dielectric Strength >= 59.1 kV/mm

@Thickness 0.0762 mm
>= 1500 kV/in

@Thickness 0.00300 in
Cured; ASTM D149