Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.2 µm/m-°C @Temperature 25.0 °C |
7.89 µin/in-°F @Temperature 77.0 °F |
|
IBC Advanced Alloys Beralcast® 363 Beryllium-Aluminum Alloy This alloy provides an ideal solution for weight, stiffness and thermal critical applications in aerospace, defense and commercial markets. BeAl-363 is a metal matrix composite which consists of 65%.. |
|||
CTE, linear | 14.2 µm/m-°C | 7.89 µin/in-°F | |
Mateck Magnesium Oxide Substrate, MgO Substrate single crystals for superconductivity |
|||
CTE, linear | 14.2 µm/m-°C | 7.89 µin/in-°F | |
Mateck MgO Substrate bicrystals for superconductivity |
|||
CTE, linear | 14.2 µm/m-°C @Temperature 25.0 - 500 °C |
7.89 µin/in-°F @Temperature 77.0 - 932 °F |
|
Wieland Simidur S 2 PFM Alloy Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |