Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wieland Simidur S 2 PFM Alloy

Category Metal , Nonferrous Metal , Precious Metal , Palladium Alloy
Manufacturer Wieland
Trade Name Simidur
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland Simidur S 2 PFM Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental
Physical Properties Metric English Comments
Density 11.2 g/cc
0.405 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 410
410
HV5/30; after porcelain firing
450
450
HV5/30; hardened
Tensile Strength, Yield 909.76 MPa

@Strain 0.200 %
131950 psi

@Strain 0.200 %
after porcelain firing
989.74 MPa

@Strain 0.200 %
143550 psi

@Strain 0.200 %
hardened
Elongation at Break 2.0 %
2.0 %
hardened
4.0 %
4.0 %
after porcelain firing
Modulus of Elasticity 122 GPa
17700 ksi
Thermal Properties Metric English Comments
CTE, linear 14.2 µm/m-°C

@Temperature 25.0 - 500 °C
7.89 µin/in-°F

@Temperature 77.0 - 932 °F
Component Elements Properties Metric English Comments
Copper, Cu 9.5 %
9.5 %
Gallium, Ga 9.0 %
9.0 %
Germanium, Ge 0.50 %
0.50 %
Gold, Au 2.0 %
2.0 %
Palladium, Pd 79 %
79 %
Processing Properties Metric English Comments
Processing Temperature 849 °C
1560 °F
Preheating Temp.
Melt Temperature 1100 - 1190 °C
2010 - 2170 °F
Casting Temperature 1340 °C
2440 °F
Descriptive Properties Value Comments
Color white