Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 90.0 - 234 µm/m-°C | 50.0 - 130 µin/in-°F | Average value: 128 µm/m-°C Grade Count:5 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |