Polymer Property : CTE, linear = 123 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 222 µm/m-°C
123 µin/in-°F
Above Tg
Tra-Con Tra-Bond F109 Fiber Optic Epoxy Adhesive
TRA-BOND F109 is specially designed to be used in fiber optic connectors where connections must be made in high humidity environments. This two part, low viscosity epoxy remains at a constant viscos..
CTE, linear 222 µm/m-°C
123 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® OG133-8 UV Cure Optical Epoxy
Material Description: A single component, UV curable, thixotropic flexible epoxy adhesive/encapsulant designed for semiconductor and opto-electronic packaging. Glob top over IC and wire bonds, and ..