Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 222 µm/m-°C | 123 µin/in-°F | Above Tg |
Tra-Con Tra-Bond F109 Fiber Optic Epoxy Adhesive TRA-BOND F109 is specially designed to be used in fiber optic connectors where connections must be made in high humidity environments. This two part, low viscosity epoxy remains at a constant viscos.. |
|||
CTE, linear | 222 µm/m-°C | 123 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® OG133-8 UV Cure Optical Epoxy Material Description: A single component, UV curable, thixotropic flexible epoxy adhesive/encapsulant designed for semiconductor and opto-electronic packaging. Glob top over IC and wire bonds, and .. |