Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 215 µm/m-°C @Temperature 24.0 - 149 °C |
119 µin/in-°F @Temperature 75.2 - 300 °F |
ASTM E831-93 |
Saint-Gobain Meldin® 5320 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
CTE, linear | 214 µm/m-°C | 119 µin/in-°F | Above Tg |
Tra-Con Tra-Cast 3104 Low Viscosity Epoxy Casting Compound TRA-CAST 3104 is a low viscosity, room temperature cure epoxy casting system developed for high performance production encapsulation and impregnating applications where filling fine intricate free s.. |
|||
CTE, linear | 215 µm/m-°C | 119 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 360ST High Temperature Epoxy Material Description: A two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications. It is a slightly th.. |