Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Meldin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Meldin® 5320 Thermoplastic Bearing Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin® 5230 BearingMeldin 5320 components supply substantial strength and rigidity. They maintain high tensile, flexural, and compressive properties, even at elevated temperatures.Applications include:Compressor Valve Plates and Valve Rings, Transmission Thrust Washers and Rings, and Vanes for Air Motors and PumpsInformation provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
ASTM D792
Water Absorption 0.11 %
0.11 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 103
103
ASTM D785
Tensile Strength 156 MPa
22600 psi
ASTM D638
Elongation at Yield 2.7 %
2.7 %
ASTM D638
Flexural Strength 250 MPa
36300 psi
ASTM D790
Flexural Modulus 9.60 GPa
1390 ksi
ASTM D790
Compressive Strength 214 MPa
31000 psi
ASTM D695
Thermal Properties Metric English Comments
CTE, linear 215 µm/m-°C

@Temperature 24.0 - 149 °C
119 µin/in-°F

@Temperature 75.2 - 300 °F
ASTM E831-93
Thermal Conductivity 0.420 W/m-K
2.91 BTU-in/hr-ft²-°F
ASTM F433
Deflection Temperature at 1.8 MPa (264 psi) 316 °C
601 °F
ASTM D648