Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 21.6 - 119 µm/m-°C | 12.0 - 66.1 µin/in-°F | Average value: 54.1 µm/m-°C Grade Count:7 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear | 0.650 - 119 µm/m-°C | 0.361 - 66.1 µin/in-°F | Average value: 92.7 µm/m-°C Grade Count:21 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |