Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 1.60 µm/m-°C @Temperature 20.0 °C |
0.889 µin/in-°F @Temperature 68.0 °F |
|
Destech Open-Celled Glassy Carbon Foam Destech glassy (vitreous) carbon foam is available in different grades depending on the number of pores per inch (ppi). Standard grades are 10, 45, 100 and 500 ppi. Custom grades are available on a.. |
|||
CTE, linear | 1.60 µm/m-°C @Temperature 20.0 - 520 °C |
0.889 µin/in-°F @Temperature 68.0 - 968 °F |
|
Advanced Ceramics ACL 2089 Cordierite Cordierite glass-ceramic has good thermal shock properties and is suitable for heat resistant components which undergo rapid thermal cycling.Information provided by Advanced Ceramics Limited (ACL) |
|||
CTE, linear | 1.60 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
0.889 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
CTE, linear | 1.60 µm/m-°C @Temperature -30.0 - 250 °C |
0.889 µin/in-°F @Temperature -22.0 - 482 °F |
average, isotropic |
AGY ZenTron® S-2 Generic S-Glass Fiber S-2 glass and S-glass have the same composition. S-glass is no longer made by AGY, but used to have a reactive epoxy size. Various silanes and starch oil are used as binders. Acid resistant. Mod.. |