Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 0.920 - 130 µm/m-°C | 0.511 - 72.0 µin/in-°F | Average value: 102 µm/m-°C Grade Count:66 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |