Polymer Property : CTE, linear = 0.450 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 0.810 µm/m-°C

@Temperature 649 °C
0.450 µin/in-°F

@Temperature 1200 °F
Pyrotek Pyrocast AR Castable Refractory
Pyrocast AR is a fused silica castable refractory inert to liquid aluminum and its alloys. It is a high strength material offering resistance to erosion and mechanical damage. Parts cast from Pyro..