Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 0.300 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 0.540 µm/m-°C

@Temperature 20.0 °C
0.300 µin/in-°F

@Temperature 68.0 °F
isotropic (axial vs. radial)
Saint-Gobain Quartzel® Fused Quartz Textiles
Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is ava..
CTE, linear 0.540 µm/m-°C

@Temperature 0.000 - 1000 °C
0.300 µin/in-°F

@Temperature 32.0 - 1830 °F
average
Saint-Gobain Spectrosil® 1000 Optical Fused Quartz
Spectrosil® 1000 grade is used for non-transmissive mirrors and substrates, and other high purity components which do not require specified optical transmission.Spectrosil® is a synthetic fuse..
CTE, linear 0.540 µm/m-°C

@Temperature 0.000 - 1000 °C
0.300 µin/in-°F

@Temperature 32.0 - 1830 °F
average
Saint-Gobain Spectrosil® 2000 Optical Fused Quartz
Spectrosil® 2000 is a deep UV, fluorescence-free grade.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually chlor..
CTE, linear 0.540 µm/m-°C

@Temperature 0.000 - 1000 °C
0.300 µin/in-°F

@Temperature 32.0 - 1830 °F
average
Saint-Gobain Spectrosil® 2100 Optical Fused Quartz
Spectrosil® 2100 has improved refractive index homogeneity.Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually c..
CTE, linear 0.540 µm/m-°C

@Temperature 0.000 - 1000 °C
0.300 µin/in-°F

@Temperature 32.0 - 1830 °F
average
Saint-Gobain Spectrosil® 2200 Optical Fused Quartz
Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 ..
CTE, linear 0.540 µm/m-°C

@Temperature 0.000 - 1000 °C
0.300 µin/in-°F

@Temperature 32.0 - 1830 °F
average
Saint-Gobain Vitreosil® 055 Optical Fused Quartz
Vitreosil® 055 is the highest grade of optical grade fused quartz available from Saint-Gobain Quartz for use in the near UV and visible. It has a useful transmission range from 270 nm in the nea..
CTE, linear 0.540 µm/m-°C

@Temperature 0.000 - 1000 °C
0.300 µin/in-°F

@Temperature 32.0 - 1830 °F
average
Saint-Gobain Vitreosil® 065 066 Optical Fused Quartz
Vitreosil® 065, for use in the near UV and visible, has a less rigorous bubble specification. It has a useful transmission range from 270 nm in the near UV to 2000 nm in the IR.Vitreosil® opt..
CTE, linear 0.540 µm/m-°C

@Temperature 0.000 - 1000 °C
0.300 µin/in-°F

@Temperature 32.0 - 1830 °F
average
Saint-Gobain Vitreosil® Clear Fused Quartz Tubing
Electrically fused quartz is recognized for its combination of purity, chemical inertness, physical stability, thermal shock resistance, high electrical resistivity, and high operating temperatures...
CTE, linear 0.540 µm/m-°C

@Temperature 0.000 - 1000 °C
0.300 µin/in-°F

@Temperature 32.0 - 1830 °F
average
Saint-Gobain Puropsil® B Infrared Grade Low [OH] Optical Fused Quartz
Puropsil® B optical infrared fused quartz is manufactured from naturally occurring quartz crystal using a plasma process to ensure a low OH. It has excellent IR transmission with a useful IR tra..
CTE, linear 0.540 µm/m-°C

@Temperature 0.000 - 1000 °C
0.300 µin/in-°F

@Temperature 32.0 - 1830 °F
average
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz
Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i..
CTE, linear 0.540 µm/m-°C

@Temperature 20.0 °C
0.300 µin/in-°F

@Temperature 68.0 °F
Cotronics Resbond™ 905 High Temperature Ceramic Adhesive, Low Expansion