Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | -6.00 µm/m-°C @Temperature 20.0 °C |
-3.33 µin/in-°F @Temperature 68.0 °F |
|
Toyobo Zylon® HM Poly(p-phenylene-2,6-benzobisoxazole) Fiber Property data below is for 1.5 denier fiber. Poly(p-phenylene-2,6-benzobisoxazole) (PBO) is a rigid-rod isotropic crystal polymer. Zylon is a new high performance fiber developed by TOYOBO using t.. |