Material Notes:
Property data below is for 1.5 denier fiber. Poly(p-phenylene-2,6-benzobisoxazole) (PBO) is a rigid-rod isotropic crystal polymer. Zylon is a new high performance fiber developed by TOYOBO using the latest material science and state of the art fiber technology. Zylon has superior tensile strength and modulus compared to p-Aramid fibers. It also has outstanding high flame resistance and thermal stability. Zylon shows excellent performance in such properties as creep, chemical resistance, cut/abrasion resistance and high temperature abrasion resistance, that far exceeds p-Aramid fibers. Zylon's moisture regain is low (0.6%) and it is dimensionally stable against humidity. Zylon is quite flexible and has a very soft hand, in spite of its extremely high mechanical properties. It can be processed into various product forms, such as continuous filament, staple fiber, spun yarn, woven and knitted fabrics, chopped fiber and pulp.Data provided by Toyobo Co., Ltd.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
Moisture Absorption at Equilibrium 0.60 %
0.60 %
at 65% RH
1.0 %
1.0 %
at 90% RH
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 5800 MPa
841000 psi
Elongation at Break 2.5 %
2.5 %
Tensile Modulus 280 GPa
40600 ksi
Tenacity 3.71 N/tex
42.0 g/denier
Thermal Properties Metric English Comments
CTE, linear -6.00 µm/m-°C

@Temperature 20.0 °C
-3.33 µin/in-°F

@Temperature 68.0 °F
Decomposition Temperature 650 °C
1200 °F
Oxygen Index 68 %
68 %
Electrical Properties Metric English Comments
Dielectric Constant 3.0

@Frequency 100000 Hz
3.0

@Frequency 100000 Hz
Dissipation Factor 0.0010
0.0010