Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 60 mm/min | 2.4 in/min | Horizontal Burning Speed 2mm thickness; ISO 3795 |
Styron Magnumâ„¢ 3525 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3525 is a resin with excellent processing characteristics. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent processability with a stable.. |
|||
Flame Spread | 60 mm/min | 2.4 in/min | Horizontal Burning Speed 2mm thickness; ISO 3795 |
Styron Magnumâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3325 MT is resin with excellent processing characteristics and a matt surface finish. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent p.. |