Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 17.8 mm/min | 0.701 in/min | ASTM D635 |
DuPont™ Surlyn® 9520 Ionomer Resin, Zinc Surlyn® 9520 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Flame Spread | 17.8 - 27.9 mm/min | 0.701 - 1.10 in/min | Average value: 23.4 mm/min Grade Count:15 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |