Thermal Properties Metric English Comments
Flame Spread 17.8 mm/min
0.701 in/min
ASTM D635
DuPont™ Surlyn® 9520 Ionomer Resin, Zinc
Surlyn® 9520 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Flame Spread 17.8 - 27.9 mm/min
0.701 - 1.10 in/min
Average value: 23.4 mm/min Grade Count:15
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..