Polymer Property : Flame Spread = 0.720 in/min
Polymer Property :
Flame Spread =
0.720 in/min
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Flame Spread
18.3
mm/min
0.720
in/min
Pass: Burn Rate- Max 100; FMVSS 302
Teknor Apex TEKRON® 4300LM-P86-1 Thermoplastic Elastomer