Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | <= 7.6 mm/min | <= 0.30 in/min | Burning Rate UL 94 HB; ASTM D635 |
Spartech Polycast Poly FR9 (0.060") Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Flame Spread | 7.6 mm/min | 0.30 in/min | VSS-302 |
Multibase Multi-Flex® A 6202 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |