Material Notes:
Description: Cell Cast AcrylicInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hr immersion
Water Absorption at Saturation 0.65 %
0.65 %
26 day immersion
Mechanical Properties Metric English Comments
Hardness, Rockwell M 96
96
ASTM D785
Tensile Strength, Yield >= 72.4 MPa
>= 10500 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Tensile Modulus 3.10 GPa
450 ksi
ASTM D638
Thermal Properties Metric English Comments
Specific Heat Capacity 1.46 J/g-°C

@Temperature 25.0 °C
0.350 BTU/lb-°F

@Temperature 77.0 °F
Dupont 900 (Therm. An. Cal.)
Flame Spread <= 7.6 mm/min
<= 0.30 in/min
Burning Rate UL 94 HB; ASTM D635
Shrinkage <= 1.0 %
<= 1.0 %
Residual Shrinkage (Internal Strain) Polycast Mil Spec; ASTM D4802
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ASTM D542
Haze <= 0.50 %
<= 0.50 %
As Cast; ASTM D1003
Transmission, Visible 92 %
92 %
As Cast; ASTM D1003
UV Transmittance 0.00 %

@Wavelength 320 nm
0.00 %

@Wavelength 320 nm
Descriptive Properties Value Comments
Smoke Density Max 13%; Rating 23.2%
ASTM D2843