Thermal Properties | Metric | English | Comments |
---|---|---|---|
Smoke Density | 1.5 min | 1.5 min | <50; ASTM E662 |
Rogers Corporation Bisco® MF1 6535 - 35 Silicone, High Performance Foam, Indentation Force Material MF1® 6535 is a high quality silicone foam material designed for a wide range of applications. It features exceptional flame, smoke and toxicity (FST) characteristics, superior weather- and UV-resi.. |
|||
Smoke Density | 1.5 min | 1.5 min | <50; ASTM E662 |
Rogers Corporation Bisco® MF1 8055 - 55 Silicone, High Performance Foam, Indentation Force Material MF1® 8055 is a high quality silicone foam material designed for a wide range of cushioning and sealing applications. It features exceptional flame, smoke and toxicity (FST) characteristics, superi.. |
|||
Smoke Density | 1.5 min | 1.5 min | <50; ASTM E662 |
Rogers Corporation Bisco® MF1 9575 - 75 Silicone, High Performance Foam, Indentation Force Material MF1® 9575 is a high quality silicone foam material designed for a wide range of cushioning and sealing applications. It features exceptional flame, smoke and toxicity (FST) characteristics, superi.. |
|||
Smoke Density | 1.5 - 1.83 min | 1.5 - 1.83 min | At 30°C; Method 4 |
Lubrizol Telene 1620 A/BK Dicyclopentadiene (DCPD) Telene® is a two-component system based on extra-high purity dicyclopentadiene (DCPD). Telene® is processed using a standard high-pressure RIM Equipment (Reaction Injection Molding). Telene® resu.. |
|||
Smoke Density | 1.5 min | 1.5 min | <20; ASTM E662 |
ACC Magnifoam™ MF1-6535™ MTI Silicones Silicone Foam Part of the Amber Chemical Group. Data provided by manufacturer. |
|||
Smoke Density | 1.5 min | 1.5 min | <20; ASTM E662 |
ACC Magnifoam™ MF1-8055™ MTI Silicones Silicone Foam Part of the Amber Chemical Group. Data provided by manufacturer. |
|||
Smoke Density | 1.5 min | 1.5 min | <20; ASTM E662 |
ACC Magnifoam™ MF1-9575™ MTI Silicones Silicone Foam Part of the Amber Chemical Group. Data provided by manufacturer. |
|||
Smoke Density | 1.5 min | 1.5 min | <20; ASTM E662 |
ACC Magnifoam™ MFSILTEC™ Roll Stock MTI Silicones Silicone Foam Part of the Amber Chemical Group. Data provided by manufacturer. |
|||
Smoke Density | 1.5 min | 1.5 min | <20; ASTM E662 |
ACC Magnifoam™ MFSILTEC™-HD MTI Silicones Silicone Foam Part of the Amber Chemical Group. Data provided by manufacturer. |
|||
Smoke Density | 1.5 min | 1.5 min | <20; D<sub>s</sub>; ASTM E662 |
Rogers Corporation Bisco® BF-2000 Ultra-Soft Silicone Foam BISCO® Ultra Soft is a highly compressible silicone foam. The combination of low weight and softness makes this flame retardant foam ideal for transportation, industrial and electronics applicatio.. |