Thermal Properties Metric English Comments
Decomposition Temperature 475 °C
887 °F
ASTM E1131
Zeus PFA Tubing
PFA, or perfluoroalkoxy, is well recognized for its ability to maintain mechanical integrity in extreme temperatures even when exposed to caustic chemicals. PFA comes in high purity versions that ar..