Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 369 °C | 696 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® 330 Low Viscosity, Optical Epoxy Product Description: EPO-TEK® 330 is a two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications.Advan.. |
|||
Decomposition Temperature | 369 °C | 696 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® OG198-54 UV Cure Optical Epoxy Material Description: Single component, low viscosity, high Tg, UV curable epoxy. Active alignment of optics, securing fibers into V-grooves and fiber pigtails are a few of its common applications... |