Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 365 °C | 689 °F | 5% weight loss; TGA; IPC-TM-650.2.4.24.6 |
Park Electrochemical Nelco® N4000-13 BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. The Nelco N4000-13 BC® is offered as a.. |
|||
Decomposition Temperature | 365 °C | 689 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® 509FM-1 General Purpose Epoxy Product Description: EPO-TEK® 509FM-1 is a two component, optically opaque epoxy designed for potting of semiconductors, PCB and systems-level electronics. It can be used in many electronic indust.. |