Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 548 °C | 1020 °F | 10% Weight Reduction |
UBE UPIMOL® R Polyimide Shape Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub.. |