Polymer Property : Decomposition Temperature = 483 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 483 °C
901 °F
TGA, Degradation Temp, uncured
Atom Adhesives AA-BOND G298 Epoxy Adhesive
AA-BOND G298 is a two component, gold-filled, electrically and thermally conductive epoxy designed for hybrid microelectronic and semiconductor packaging.Appearance: Resin: Brown, Hardener: Dark Bro..