Thermal Properties Metric English Comments
Decomposition Temperature 428 °C
802 °F
Degradation Temperature; TGA
Epoxy Technology EPO-TEK® E2001 Electrically Conductive, Silver-Filled Epoxy
Product Description: EPO-TEK® E2001 is a two component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications using a snap-cure profile. Advantages & Appl..
Decomposition Temperature 428 °C
802 °F
Degradation Temperature; TGA
Epoxy Technology EPO-TEK® E3001 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® E3001-HV is a snap cure, single component, silver-filled die attach adhesive for semiconductor plastic IC packaging. Also available in a frozen syringe. Advantages & ..