Thermal Properties Metric English Comments
Decomposition Temperature 403 °C
757 °F
Degradation Temperature
Epoxy Technology EPO-TEK® ED1021 Epoxy
Preliminary Product Information SheetMaterial Description: A single component, silver-filled epoxy designed for low power semiconductor LED die attach applications. Unique features include its abil..