Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 295 °C | 563 °F | Onset; IPC TM-650 2.3.41 |
Arlon 47N Quick Cure Epoxy Low-Flow Prepreg 47N is a low-flow epoxy prepreg engineered for binding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. An optional low lamination temperature protects components already mou.. |