Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 200 °C | 392 °F | Heat Stability |
PolyOne OnColor™ 30BKA488 Black Polyvinyl Chloride, Unspecified (PVC, Unspecified) Dispersion Note: On a scale in which 1 represents an excellent dispersion and 5 a poor dispersion. Heat Stability Note: Under normal processing conditions there is normally no significant color chan.. |
|||
Decomposition Temperature | 200 °C | 392 °F | |
H.C. Starck Baymetec® Niobium Ethoxide |
|||
Decomposition Temperature | >= 200 °C | >= 392 °F | Thermal stability, for 80 minutes |
Sibur 1030-13 Compound OMN Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |