Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne OnColor™ 30BKA488 Black Polyvinyl Chloride, Unspecified (PVC, Unspecified)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name OnColor™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne OnColor™ 30BKA488 Black Polyvinyl Chloride, Unspecified (PVC, Unspecified).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dispersion Note: On a scale in which 1 represents an excellent dispersion and 5 a poor dispersion. Heat Stability Note: Under normal processing conditions there is normally no significant color change at the temperature indicated. Volume Resistivity Note: Measured with 1% concentrate mixed with natural PVC having a volume resistivity of greater than 1x10 exp14 ohm-cm.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Density 0.625 g/cc
0.0226 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
10 sec; ASTM D2240
Thermal Properties Metric English Comments
Decomposition Temperature 200 °C
392 °F
Heat Stability
Electrical Properties Metric English Comments
Volume Resistivity 1.0 ohm-cm
1.0 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Moisture Content <= 0.30 %
<= 0.30 %
Descriptive Properties Value Comments
Appearance Cubes
ASTM D2090
Forms Cube
Pellets
Generic Material PVC, Unspecified
Generic Name Polyvinyl Chloride, Unspecified (PVC, Unspecified)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Insulation
Wire & Cable Applications