Polymer Property : Decomposition Temperature = 185 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature >= 185 °C
>= 365 °F
Thermal stability, for 120 minutes
Sibur L-85M Polyvinyl Chloride (PVC)
For use in the footwear industry for production of shoe soles.
Decomposition Temperature >= 185 °C
>= 365 °F
Thermal stability, for 90 minutes
Sibur PL-1GS Polyvinyl Chloride (PVC)
For the production of boot tops and soles of autumn-spring purpose and for production of boots by molding method under pressure.
Decomposition Temperature >= 185 °C
>= 365 °F
Thermal stability, for 90 minutes
Sibur PL-2PS Polyvinyl Chloride (PVC)
For the production of boot tops and soles of autumn-spring purpose and for production of boots by molding method under pressure.
Decomposition Temperature >= 185 °C
>= 365 °F
Thermal stability, for 35 minutes
Sibur PPSH Polyvinyl Chloride (PVC)
For production of irrigation hoses.
Decomposition Temperature 185 - 200 °C
365 - 392 °F
Average value: 188 °C Grade Count:5
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..