Sibur PPSH Polyvinyl Chloride (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Sibur
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sibur PPSH Polyvinyl Chloride (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For production of irrigation hoses.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 16.0 MPa
>= 2320 psi
Elongation at Break >= 300 %
>= 300 %
Thermal Properties Metric English Comments
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
Decomposition Temperature >= 185 °C
>= 365 °F
Thermal stability, for 35 minutes