Thermal Properties Metric English Comments
Flash Point 6.50 °C
43.7 °F
3M 4296T Adhesion Promoter
3MTM Adhesion Promoter 4296T is a liquid primer for flexible high solids paints and raw RIM. It is specifically formulated to be used with 3MTM Acrylic Foam Tapes for automotive applications.Informa..
Flash Point 6.50 °C
43.7 °F
BASF DMF-DM 1,1-Dimethoxy-N,N-dimethyl methanamine
Formula: C5H13NO2CAS: 4637-24-5Description: DMF-DMA is a colorless to yellow liquid, with an ether-like odor. In water is spontaneously decomposes and is soluble in organic solvents.Synonyms: DMF-D..
Flash Point 6.50 °C
43.7 °F
BASF Propionyl Chloride
Formula: C3H5ClOCAS: 79-03-8Description: Propionyl chloride is a colorless to light yellow liquid with a pungent odor. It hydrolyses in the presence of water.Synonyms: Propanoyl chloride, Propionic..
Copyright © lookpolymers.com All Rights Reserved