Material Notes:
Formula: C5H13NO2CAS: 4637-24-5Description: DMF-DMA is a colorless to yellow liquid, with an ether-like odor. In water is spontaneously decomposes and is soluble in organic solvents.Synonyms: DMF-DMAApplications: Intermediate used in the production of Pharmaceuticals.Information provided by BASF
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
Molecular Weight 119.2 g/mol
119.2 g/mol
Thermal Properties Metric English Comments
Boiling Point 104 - 108 °C
219 - 226 °F
Flash Point 6.50 °C
43.7 °F
Descriptive Properties Value Comments
Assay >96%
Ignition Temperature 155°C