Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 52.2 °C | >= 126 °F | |
Parker Chomerics CHO-FLEX 4434P Conductive Adhesive Information provided by Chomerics |
|||
Flash Point | 52.2 °C | 126 °F | Seta, Closed Cup |
Lord Adhesives Chemglaze® 9956 Airless Spray Thinner Chemglaze® thinners are formulated with urethane grade solvents and are used to reduce viscosity, aid bubble release, minimize orange peel, and make application easier.Chemglaze 9974 additive is .. |