Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Volatiles 40 %
40 %
Thermal Properties Metric English Comments
Flash Point >= 52.2 °C
>= 126 °F
Component Elements Properties Metric English Comments
Copper, Cu <= 50 %
<= 50 %
Silver, Ag <= 5.0 %
<= 5.0 %
Descriptive Properties Value Comments
2-Ethoxyethylacetate wt. % Max 40
Epoxy Resin, wt % < 5
Formaldehyde wt. % 0.6
Phenolic Resin wt. % Max 10
Physical Form Gray viscous liquid with mild odor.
Polyester Resins wt. % <20
Silicone Resin % <5
Copyright © lookpolymers.com All Rights Reserved