Thermal Properties Metric English Comments
Flash Point 264 °C
507 °F
ASTM D92
ExxonMobil 100 Exxon Aviation Oil
Aviation Oil 100, 120 and 20W-50 are  non-dispersant, mineral oil-based lubricants for piston engines of commercial, military and private aircraft. They contain very low concentrations of anti-oxid..
Flash Point 264 °C
507 °F
ExxonMobil Diol 13 RD 40
DIOL railroad oils are a full line of heavy-duty crankcase lubricants for locomotive diesel engines. These products are designed to meet the severe service demands imposed by newer railroad diesel l..
Flash Point 264 °C
507 °F
ASTM D92
ExxonMobil Mobil Pegasus 610 40
Mobil Pegasus 610 is a high performance natural gas engine oil primarily intended for the lubrication of modern medium and high speed four-cycle engines operating on fuel that contains corrosive mat..
Flash Point 264 °C
507 °F
ASTM D92
ExxonMobil 50 Exxon XD-3
Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d..
Flash Point 264 °C
507 °F
ASTM D92
ExxonMobil Mobil Rarus 427
The Mobil Rarus 400 Series is a line of premium performance ashless air compressor lubricants designed to meet the stringent requirements of the major compressor manufacturers. They are formulated w..
Flash Point 264 °C
507 °F
ASTM D92
ExxonMobil Mobil Vaculine 525
Mobil Vacuoline 500 Series are extra high performance heavy duty circulating oils specifically designed to meet the critical requirements of the Morgan Construction Companys high speed No-Twist® Ro..
Flash Point 264 °C
507 °F
ChevronTexaco 220 Way Lubricant
Texaco Way Lubricants deliver value through:Excellent separation from metalworking coolants — The SKC (SKC Gleittechnik) coolant separation test showed excellent separation from a wide variety of c..
Flash Point 264 °C
507 °F
ASTM D92
ChevronTexaco 600 White Oil
FeaturesChevron Technical White Oils are high quality, highly refined, odorless, tasteless, clear, paraffinic, technical grade white oils.Chevron Technical White Oils are hydrocracked and dewaxed us..
Flash Point 264 °C
507 °F
ChevronTexaco Canopus® 100
Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant ..
Flash Point 264 °C
507 °F
ASTM D92
ChevronTexaco ISO 100 Utility Oil HVI
FeaturesChevron Utility Oil HVI is a high quality, high viscosity index uncompounded oil with excellent water separating characteristics.Chevron Utility Oil HVI possesses good natural thermal and ox..
Flash Point 264 °C
507 °F
ASTM D92
ExxonMobil 100 Exxon Aviation Oil
Aviation Oil 100, 120 and 20W-50 are  non-dispersant, mineral oil-based lubricants for piston engines of commercial, military and private aircraft. They contain very low concentrations of anti-oxid..
Flash Point 264 °C
507 °F
ASTM D92
ExxonMobil Mobil Rarus 427
The Mobil Rarus 400 Series is a line of premium performance ashless air compressor lubricants designed to meet the stringent requirements of the major compressor manufacturers. They are formulated w..
Flash Point 264 °C
507 °F
ASTM D92
ExxonMobil Mobil Vaculine 525
Mobil Vacuoline 500 Series are extra high performance heavy duty circulating oils specifically designed to meet the critical requirements of the Morgan Construction Companys high speed No-Twist® Ro..
Flash Point 264 °C
507 °F
ASTM D92
ChevronTexaco Clarity® ISO 100 Synthetic Paper Machine Oil
FeaturesChevron Clarity Synthetic Paper Machine Oils combine the unique ashless formulation of Chevron Clarity® Paper Machine Oils with the superior performance properties of polyalphaolefin (PAO) ..
Flash Point 264 °C
507 °F
ASTM D92
ChevronTexaco Vistac® ISO 220 Way Oil D
FeaturesChevron Way Oils Vistac D are high quality lubricants designed to meet the critical lubrication demands for the slides and ways of machine tools.Chevron Way Oils Vistac D is formulated with ..
Flash Point 264 °C
507 °F
ASTM D92
ExxonMobil 50 Exxon XD-3
Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d..
Flash Point 264 °C
507 °F
ExxonMobil Diol 13 RD 40
DIOL railroad oils are a full line of heavy-duty crankcase lubricants for locomotive diesel engines. These products are designed to meet the severe service demands imposed by newer railroad diesel l..
Flash Point 264 °C
507 °F
ASTM D92
ExxonMobil Mobil Pegasus 610 40
Mobil Pegasus 610 is a high performance natural gas engine oil primarily intended for the lubrication of modern medium and high speed four-cycle engines operating on fuel that contains corrosive mat..