ExxonMobil Mobil Pegasus 610 40

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Mobil Pegasus 610 40.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mobil Pegasus 610 is a high performance natural gas engine oil primarily intended for the lubrication of modern medium and high speed four-cycle engines operating on fuel that contains corrosive materials such as hydrogen sulphide or halogens (compounds containing chlorine, fluorine, etc.). These engines are generally of the lean-burn design where increased manifold pressures prevent sufficient lubricant from reaching the valve guide areas resulting in low oil consumption which can lead to accelerated valve guide and valve recession. This effect also increases the potential for wear and acid attack of upper cylinder components from the acidic materials generated during combustion. The Mobil Pegasus 610 is a 1.0% ash, high TBN gas engine oil with exceptional reserve alkalinity designed to offset the negative effects of these corrosive materials on engine components. The excellent corrosion protection properties prevent corrosive wear in cylinders, valve areas and bearings which can result in longer engine life and lower maintenance costs. Mobil Pegasus 610 provides excellent anti-wear and anti-scuff performance assuring minimal piston scuffing, scoring and cylinder and ring wear. This oil can also be used for the lubrication of the reciprocating compressors in landfill and biomas gas applications. Mobil Pegasus 610 is formulated from high quality mineral base oils combined with an advanced technology 1.0% ash additive system designed to provide excellent protection of engine and compressor components. This product exhibits a high level of chemical stability and resistance to oxidation and nitration. Mobil Pegasus 610 offers outstanding resistance to valve train wear and protection against deposit and sludge formation. These performance advantages combined with the very effective detergency and dispersancy characteristics control the formation of ash and carbon deposits that could result in poor engine performance and detonation.Gas engines operating on fuel that contains moderate levels of hydrogen sulphide (H2S); Engines operating on fuel containing other corrosive components such as TOHCl (Total Organic Halides as Chloride); Spark ignited four-stroke cycle gas engines with very low oil consumption; Reciprocating compressors operating on natural gas that contains sulphur or halogens; High output or naturally aspirated engines operating at or in excess of rated capacity under high temperatures
Physical Properties Metric English Comments
Density 0.890 g/cc

@Temperature 15.6 °C
0.0322 lb/in³

@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 102
102
Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 130 cSt
130 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 13.8 cSt
13.8 cSt
ASTM D445
Ash <= 0.98 %
<= 0.98 %
Sulfated Ash, wt%; ASTM D874
Thermal Properties Metric English Comments
Pour Point -18.0 °C
-0.400 °F
ASTM D97
Flash Point 264 °C
507 °F
ASTM D92
Chemical Properties Metric English Comments
Total Base Number 8.6
8.6
mgKOH/g; ASTM D2896