Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 261 °C | 502 °F | ASTM D92 |
ExxonMobil Teresstic 100 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Flash Point | >= 261 °C | >= 502 °F | |
Westlake Epolene® C-16 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed, Chemically Modified Product Description: Epolene C-16 is a branched low density polyethylene modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersions, and.. |
|||
Flash Point | >= 261 °C | >= 502 °F | |
Westlake Epolene® C-16P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer Description: Epolene C-16P is a branched low density polyethylene powder modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersions, and.. |
|||
Flash Point | >= 261 °C | >= 502 °F | |
Westlake Epolene® C-18 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed, Chemically Modified Product Description: Epolene C-18 is a branched low density polyethylene modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersion, and .. |
|||
Flash Point | >= 261 °C | >= 502 °F | |
Westlake Epolene® C-18P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer Description: Epolene C-18P is a branched low density polyethylene powder modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersion, and .. |
|||
Flash Point | >= 261 °C | >= 502 °F | |
Westlake Epolene® C-19 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed Product Description: Epolene C-19 is a branched low density polyethylene modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersion, and .. |
|||
Flash Point | 261 °C | 502 °F | ASTM D92 |
ExxonMobil Teresstic 100 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |