Westlake Epolene® C-18 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed, Chemically Modified

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Westlake Chemical Corporation
Trade Name Epolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Epolene® C-18 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed, Chemically Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Epolene C-18 is a branched low density polyethylene modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersion, and applications requiring compatibility with polyamide. Coatings produced with Epolene C-18 exhibit high gloss, low moisture vapor transmission rates, grease resistance, and good heat seal ability. In hot melt adhesives, the maleic anhydride modification allows for improved adhesion, greater filler tolerance, broader capabilities, and improved aging properties.Key Attributes:Enhances paraffin wax coating properties like gloss, grease resistance, and MVTR Excellent thermal stabilityMaleic anhydride grafted PE provides functionalityMedium molecular weightUseful in color concentratesApplication/Uses:Automotive OEMAutomotive refinishAutomotiveBuilding and ConstructionHot Melt AdhesivesPackagingSolvent borne Adhesives
Physical Properties Metric English Comments
Specific Gravity 0.890 - 0.920 g/cc
0.890 - 0.920 g/cc
Viscosity 2400 - 6000 cP

@Temperature 150 °C
2400 - 6000 cP

@Temperature 302 °F
542-111
Brookfield Viscosity 1550 cP

@Temperature 190 °C
1550 cP

@Temperature 374 °F
ASTM D3226
7750 cP

@Temperature 125 °C
7750 cP

@Temperature 257 °F
ASTM D3226
Molecular Weight 15000 g/mol
15000 g/mol
Thermal Properties Metric English Comments
Flash Point >= 261 °C
>= 502 °F
Ring & Ball Softening Point 101 °C
214 °F
ASTM E28
Optical Properties Metric English Comments
Gardner Color Number >= 1.0
>= 1.0
542-130
Chemical Properties Metric English Comments
Total Acid Number 1.5 - 2.5
1.5 - 2.5
542-110
Descriptive Properties Value Comments
Penetration Hardness 4 dmm
ASTM D5, Needle under 100-g load for 5s @ 25°C, tenths of mm