Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 43.3 °C | 110 °F | M1433B; Setaflash, Closed Cup; ASTM D3278-82 |
Lord Adhesives Aeroglaze® M1433 Elastomeric Polyurethane Rain Erosion Coating Aeroglaze® M1433 elastomeric coating functions exceptionally well in abrasive environments. Inherent flexibility, corrosion resistance, and energy absorptive properties make Aeroglaze M1433 elast.. |
|||
Flash Point | 43.3 °C | 110 °F | Part B, M201; Setaflash |
Lord Adhesives Chemglaze® M331 Elastomeric Polyurethane Chemglaze® M331 is a two package, ASTM D-16 Type IV elastomeric polyurethane coating. Cured films produced from this coating are tough, flexible, and resistant to erosion, abrasion, and impact. T.. |