Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 4.40 °C | 39.9 °F | Tag Closed Cup |
LyondellBasell TBAcâ„¢ Solvent, Tertiary butyl acetate Information provided by Lyondell. |
|||
Flash Point | 4.40 °C | 39.9 °F | closed cup |
Dow Corning SYL-OFF® 7362 COATING Syl-Off® 7362 Coating is a 30% solids dispersion of vinyl functional silicone polymer in toluene. A pre-catalysed coating suitable for fast cure applications, recommended for use with 7367 Crosslin.. |
|||
Flash Point | 4.40 °C | 39.9 °F | |
Dow Corning SYL-OFF® PMCP7362 Coating Syl-Off® 7362 Coating is a 30% solids dispersion of vinyl functional silicone polymer in toluene. A pre-catalysed coating suitable for fast cure applications, recommended for use with 7367 Crosslin.. |
|||
Flash Point | 4.40 °C | 39.9 °F | closed cup |
Dow Corning Z-1227 METHYLVINYLDICHLOROSILANE Information provided by Dow Corning |
|||
Flash Point | 4.40 °C | 39.9 °F | |
3M K500 Adhesion Promoter 3M™ Adhesion Promoter K500 is a liquid promoter used for most ethylene propylene diene monomer (EPDM), polypropylene (PP), chlorinated rubbers, acrylonitrile butadiene styrene (ABS) and certain pol.. |