Material Notes:
3M™ Adhesion Promoter K500 is a liquid promoter used for most ethylene propylene diene monomer (EPDM), polypropylene (PP), chlorinated rubbers, acrylonitrile butadiene styrene (ABS) and certain polyethylene terephthalate (PET)/polybutylene terephthalate (PBT) blends.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 8.0 %
8.0 %
Thermal Properties Metric English Comments
Flash Point 4.40 °C
39.9 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
date of receipt by customer
Descriptive Properties Value Comments
Appearance Straw