Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 188 °C | 370 °F | |
Lubriplate FMO 150 AW USP Mineral Oil-Based Food Machinery Grade Oil For use where a Class H-1 oil is required. Manufactured in nine ISO grades for a variety of applications. Anti-wear fortified. NOTE: FMO-350AW is also available in a red and orange color which helps.. |
|||
Flash Point | 188 °C | 370 °F | ASTM D92 |
ExxonMobil 11M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Flash Point | 188 °C | 370 °F | ASTM D92 |
ExxonMobil 12M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Flash Point | 188 °C | 370 °F | ASTM D92 |
ChevronTexaco ISO 150 Marine Oil E FeaturesChevron Marine Oils E are formulated using a blend of high grade, medium viscosity index base oils and carefully balanced additive package to meet the crankcase need of marine steam engines... |
|||
Flash Point | 188 °C | 370 °F | ASTM D92 |
ChevronTexaco ISO 32 Utility Oil LVI FeaturesChevron Utility Oils LVI are general purpose lubricants. Chevron Utility Oils LVI are light-colored oils that possess excellent natural low pour points, along with low carbon-forming tendenc.. |
|||
Flash Point | 188 °C | 370 °F | |
ChevronTexaco Rando® HDZ 22 Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor.. |
|||
Flash Point | 188 °C | 370 °F | ASTM D92 |
ChevronTexaco Regal® N-68 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |
|||
Flash Point | 188 °C | 370 °F | ASTM D92 |
ExxonMobil 11M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Flash Point | 188 °C | 370 °F | ASTM D92 |
ExxonMobil 12M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Flash Point | >= 188 °C | >= 370 °F | ASTM D92 |
ExxonMobil Mobil Almo 525 Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio.. |
|||
Flash Point | 188 °C | 370 °F | |
ConocoPhillips Conoflex® 32 SRI Lubricant ISO Description: Conoco Conoflex SRI Lubricant is an excellent wire rope lubricant and preservative for any metal product, particularly when protecting from saltwater. It lubricates and preserves the wi.. |
|||
Flash Point | 188 °C | 370 °F | |
ConocoPhillips Hydroclear® 15 Spindle Oil Description: Conoco Hydroclear Spindle Oil is a high-quality needle- and spindlebearing lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Spindle Oil is specially formula.. |
|||
Flash Point | 188 °C | 370 °F | ASTM D92 |
ChevronTexaco Superla® 10 White Oil FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch.. |
|||
Flash Point | 188 °C | 370 °F | |
ConocoPhillips Hydroclear® V Automatic Transmission Fluid Description: Conoco Hydroclear MERCON V Automatic Transmission Fluid is a premium multifunctional product that has been approved for use in all General Motors and Ford transmissions. It carries both.. |
|||
Flash Point | >= 188 °C | >= 370 °F | ASTM D92 |
ExxonMobil Mobil Almo 525 Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio.. |
|||
Flash Point | 188 °C | 370 °F | |
ChevronTexaco Alcaid® 32 Texaco Alcaid® oils deliver value through:Low pour points that permit oils to remain fluid at subzero temperatures.Ready separation from water, an important property where severe moisture condition.. |