Polymer Property : Flash Point = 188 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 188 °C
370 °F
Lubriplate FMO 150 AW USP Mineral Oil-Based Food Machinery Grade Oil
For use where a Class H-1 oil is required. Manufactured in nine ISO grades for a variety of applications. Anti-wear fortified. NOTE: FMO-350AW is also available in a red and orange color which helps..
Flash Point 188 °C
370 °F
ASTM D92
ExxonMobil 11M Mobil DTE 10M Series
Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and ..
Flash Point 188 °C
370 °F
ASTM D92
ExxonMobil 12M Mobil DTE 10M Series
Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and ..
Flash Point 188 °C
370 °F
ASTM D92
ChevronTexaco ISO 150 Marine Oil E
FeaturesChevron Marine Oils E are formulated using a blend of high grade, medium viscosity index base oils and carefully balanced additive package to meet the crankcase need of marine steam engines...
Flash Point 188 °C
370 °F
ASTM D92
ChevronTexaco ISO 32 Utility Oil LVI
FeaturesChevron Utility Oils LVI are general purpose lubricants. Chevron Utility Oils LVI are light-colored oils that possess excellent natural low pour points, along with low carbon-forming tendenc..
Flash Point 188 °C
370 °F
ChevronTexaco Rando® HDZ 22
Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor..
Flash Point 188 °C
370 °F
ASTM D92
ChevronTexaco Regal® N-68 R&O
Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high..
Flash Point 188 °C
370 °F
ASTM D92
ExxonMobil 11M Mobil DTE 10M Series
Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and ..
Flash Point 188 °C
370 °F
ASTM D92
ExxonMobil 12M Mobil DTE 10M Series
Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and ..
Flash Point >= 188 °C
>= 370 °F
ASTM D92
ExxonMobil Mobil Almo 525
Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio..
Flash Point 188 °C
370 °F
ConocoPhillips Conoflex® 32 SRI Lubricant ISO
Description: Conoco Conoflex SRI Lubricant is an excellent wire rope lubricant and preservative for any metal product, particularly when protecting from saltwater. It lubricates and preserves the wi..
Flash Point 188 °C
370 °F
ConocoPhillips Hydroclear® 15 Spindle Oil
Description: Conoco Hydroclear Spindle Oil is a high-quality needle- and spindlebearing lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Spindle Oil is specially formula..
Flash Point 188 °C
370 °F
ASTM D92
ChevronTexaco Superla® 10 White Oil
FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch..
Flash Point 188 °C
370 °F
ConocoPhillips Hydroclear® V Automatic Transmission Fluid
Description: Conoco Hydroclear MERCON V Automatic Transmission Fluid is a premium multifunctional product that has been approved for use in all General Motors and Ford transmissions. It carries both..
Flash Point >= 188 °C
>= 370 °F
ASTM D92
ExxonMobil Mobil Almo 525
Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio..
Flash Point 188 °C
370 °F
ChevronTexaco Alcaid® 32
Texaco Alcaid® oils deliver value through:Low pour points that permit oils to remain fluid at subzero temperatures.Ready separation from water, an important property where severe moisture condition..